Selected job
Live outdoorsSun, rain, a hot car
UV stability and heat resistance for parts that leave the workshop and stay outside.
Grades that fit
5 grades can hold it.
The same catalogue read along the job: each grade with its heat deflection, its chamber requirement and the thing to watch when printing it.
| Grade | Family | Heat deflection | Chamber | Watch out |
|---|---|---|---|---|
| PETG Core | PETG | 76–78 °C | Optional | Sticks to smooth PEI hard enough to pull chips out. Use a textured plate or glue as a release layer. |
| PETG-CF | PETG | 68,6 °C | Optional | Fibre lowers elongation from 18 % to around 6 %. Do not use it for living hinges. |
| ASA Core | ABS/ASA | 103 °C | 50–60 °C | Same warping and ventilation rules as ABS. Do not print it in an open room. |
| PA6-GF | Nylon | 191 °C | 55 °C | Glass fibre is harder on nozzles than carbon. Budget for a wear part, not a permanent one. |
| PC Core | PC | 111–114 °C | 50–60 °C | Delaminates if you print it too cool. Under 260 °C the layers never properly fuse. |
The properties on this page are values published in the named manufacturers' data sheets, measured on their grades to the standard printed against each row — not measurements of a ZORVA spool. Use them to compare material classes, not as an acceptance specification.
Matches
4 families can do this.
Listed without ranking. The cheapest grade that clears your requirement is usually the right one.
Glycol-modified polyethylene terephthalate
PETG
Impact tolerant and water resistant. Stringy if you print it wet or fast.
- SKUs
- 5
- Heat
- 76–78 °C
- Price
- On request
Acrylonitrile butadiene styrene / acrylonitrile styrene acrylate
ABS & ASA
Heat resistant and UV stable (ASA). Warps without an enclosure.
- SKUs
- 5
- Heat
- 100–106 °C
- Price
- On request
Polyamide, carbon and glass reinforced
Nylon & composites
The best fatigue and wear performance available on an FDM printer. Needs a dryer.
- SKUs
- 3
- Heat
- 215 °C
- Price
- On request
Polycarbonate and PC blends
Polycarbonate
Highest strength and heat resistance here. Also the least forgiving.
- SKUs
- 3
- Heat
- 111–114 °C
- Price
- On request
Grades
11 SKUs for this job
PETG Core
Natural
Light passes through — useful for level windows and diffusers.
PETG Core
Steel Grey
The technical grey from the ZORVA palette. Hides scuffs on shop parts.
PETG Core
Signal Orange
For guards, handles and anything that should be obvious in a machine.
PETG Core
Graphite
Standard housing colour. Takes a vapour-free polish with fine abrasive.
PETG-CF
Onyx
Matte straight off the plate. Fibre also cuts stringing to almost nothing.
ASA Core
Slate Grey
Holds colour in direct sun where grey PLA chalks out within a season.
ASA Core
Arctic White
Reflects heat, which matters for sensor housings in the sun.
ASA Core
Signal Orange
UV-stable orange for outdoor markers and safety hardware.
PA6-GF
Slate
Glass fibre shows as a fine speckle. It is the material, not a print defect.
PC Core
Clear
Transparent tinted as printed. Water clear needs thin layers and near-zero cooling.
PC Core
Graphite
Structural PC where transparency is irrelevant and cost is not.